Cementitemicrostructure

About Viking Drill and Tool Viking Drill and Tool begins with the finest tool steel we can buy and ends with the world class products in our catalog. Our cutting tools are designed, engineered and superbly crafted to provide long lasting durability.

For a eutectoid steel, describe isothermal heat treatments that would be required to yield specimens having the following Brinell hardnesses: (a) \(180 \mathrm{HB}\) (b) \(220 \mathrm{HB}\), and (c) 500 HB.

Image

Ferrite andpearlite microstructure

The kinetics of the austenite-to-pearlite transformation obey the Avrami relationship. Using the fraction transformed-time data given here, determine the total time required for \(95 \%\) of the austenite to transform to pearlite: $$\begin{array}{cc} \hline \text {Fraction Transformed} & \text {Time (s)} \\ \hline 0.2 & 280 \\ 0.6 & 425 \\ \hline \end{array}$$

Bainitemicrostructure

Briefly cite the differences between pearlite, bainite, and spheroidite relative to microstructure and mechanical properties

Ferritemicrostructure

Briefly explain why fine pearlite is harder and stronger than coarse pearlite, which in turn is harder and stronger than spheroidite.

Image

Image

Rank the following iron-carbon alloys and associated microstructures from the hardest to the softest: (a) 0.25 wt\% C with coarse pearlite, (b) 0.80 wt\% \(C\) with spheroidite, (c) \(0.25 \mathrm{wt} \% \mathrm{C}\) with spheroidite, and (d) 0.80 wt\% C with fine pearlite. Justify this ranking.