“A simple example of this would be 50 per cent of the material taken away by voids or interruptions at the surface,” he said. “Fifty per cent of the surface remains in contact with the tool compared to an interrupted part. So, in this case, double the SFM to compensate for that.”
“For roughing applications, I would like to have a tougher grade with a larger T-land or a roughing chipbreaker with a nice edge prep to maintain the interruptions as well as hold that dimensional tolerance,” said Haid. “When finishing, go with something harder rather than something tougher to hold the tolerance and not wear out as fast.”
For interrupted cuts in softer or more ductile materials, having an edge prep with a larger or wider land is a good option. With ceramic, the insert does not need to be as negative as it would for a harder material; with carbide, a medium-duty chip form will provide additional shear, which is beneficial in most cases.
Speeds and Feeds. The experts agree that one of the biggest mistakes an operator can make during interrupted turning is to reduce speed.
“For interrupted-style cuts on hardened material, it’s best to choose heavier edge preparations,” said Goss. “With ceramic, having a large single or compound chamfer/land, or with carbide, having a heavier-duty chip form, will ensure the insert is able to handle the abusive nature of the cut and redirect those forces appropriately to allow for maximum tool life.”
Choosing the right grade depends on the type and hardness of the material, as well as the level of interruption and the machining stage, whether roughing or finishing.
At the recent AMB 2024 exhibition in Stuttgart, Matthew Farnsworth, commercial director at the University of Sheffield Advanced Manufacturing Research Centre (AMRC) announced that CNC machining centres manufacturer, Heller has become its latest tier 1 member.
Choosing the right insert for interrupted turning can make all the difference in success of the overall process. One of the big misconceptions is that operators can just use whatever insert is available. Sometimes this may work out, but often operators will struggle.
Luminoso has a bachelor of arts from Carleton University, a bachelor of education from Ottawa University, and a graduate certificate in book, magazine, and digital publishing from Centennial College.
“PVD coatings have a thin layer that really holds up better against the impacts of interruptions versus the CVD option,” said Haid.
Formerly a user could select a grooving width of either 5, 6 or 8mm, but now smaller inserts with a cutting width of 3 or 4mm are available. In the UK and Ireland, the tools are supplied through the German manufacturer's subsidiary in Ringwood, Hampshire.
“Although positive inserts are generally not recommended for interrupted cuts, sometimes they are unavoidable,” said Mitchell. “In situations such as these, it is highly recommended to use a double-sided positive insert. Traditional positive inserts sit in a pocket and the only thing preventing them from moving is a small screw. But [some inserts] utilize a dovetail pocket, ensuring no movement even in interrupted applications, while still providing a positive cutting action.”
The M475 system employs precision-ground, indexable inserts with four cutting edges. Positive geometry and a round chip breaker groove together with a new carbide grade, RC4G, deliver economical, productive machining performance. High toughness and hardness enable the machining of steels at elevated cutting speeds and also leads to significantly increased insert life. The cutter bodies are supplied from stock as side, shell and screw-in milling cutters, the two latter variants being equipped for internal coolant supply.
With carbide grades, having either a large grain size or cobalt-enriched layer as part of the substrate will make for a stronger insert. Larger carbide grains have more impact on strength compared to a fine-grade carbide.
LOGIQ 6 Turn. NEW Unique 6 Positive Cutting Edged Insert Shape Designed for Superior Finishing, Featuring 6 Cutting Edges that Provide Excellent Surface Finish.
“Basically, you want to look for the strongest insert possible,” said Paul Lobsinger, sales and service engineer Canada, Greenleaf Corp. “It helps to have a tough negative insert to accept the interruptions and pounding.”
“The benefit of dealing with interrupted cuts in the roughing stage is that the insert can be changed, from part to part, without an offset,” said Matthew Haid, application specialist, Dormer Pramet, Mississauga, Ont. “Dealing with interrupted cuts in finish-turning can be much more challenging. If the part has a tight finishing tolerance, operators typically need to adjust the tool wear offset on the CNC over the course of the insert’s life. When changing the insert, it's recommended not to start at zero or the regular offset, but rather do a first pass to confirm the tolerance dimension. Both interrupted roughing and finishing can be a challenge, but with roughing, there is always material left to be finished, whereas finishing tends to be more sensitive.”
“Most commonly, an interruption is a break in the continuity of the material during the machining process,” said Matt Goss, applications engineer and project development, Greenleaf Corp., Saegertown, Pa. “This is where the insert engages and disengages with the workpiece, either once or a series of times. These interruptions can either be induced as part of the machining process, such as turning over bolt circles or holes, slots, or keyways, or they can be inherent to the workpiece, for example if it is out of round or has forging scale on the surface. Each of these cases presents a scenario where there's a break in continuous and uniform flow of material across the cutting tool.”
The experts noted that some operators tend to favour a positive geometry as they think it will help take the impact, but that is just not the case. A negative geometry is going to provide a much better cut in interrupted turning.
Interrupted cutting in turning is subjective. While some operators may look at a part with a keyway and a small depth of cut as a heavy interruption, another operator may classify heavy interruptions only as multiple interruptions with a larger depth of cut. The workpiece material, part configuration and features, and depth of cut will all come into play when determining how the interruption will affect the overall process.
“There needs to be a balance,” said Goss. “You don't want to have too much negativity or a large land on some of those soft, ductile materials, which could lead to excessive cutting force. But it also needs to be heavy enough to provide adequate performance and tool life.”
Optimal strength is going to be realized by using a round geometry and a negative-style insert. Mitchell also noted that it’s important to pay attention to the chipbreaker selection. Some chipbreakers are designed for heavy interruptions, but others are designed to be free cutting and as sharp as possible, making them fragile and prone to chipping in an interrupted application.
“However, coolant should almost always be shut off, unless machining an extremely gummy material,” said Mitchell. “When coolant is applied to an insert machining an interrupted cut, the insert undergoes extreme heat, then no heat when encountering the interruption. The hot insert is then suddenly submerged in coolant, which causes thermal cracking, shortening the tool life and potentially causing catastrophic failure.”
With interrupted cuts there is a greater risk for the cutting edge to break down prematurely or inconsistently, lowering part quality. It is important to choose the best cutting tool and process parameters during interrupted turning operations. Phuchit/iStock/Getty Images Plus
Cutting tool manufacturer Horn has extended downwards in size its M475 grooving and cut-off milling system. Formerly a user could select a grooving width of either 5, 6 or 8mm, but now smaller inserts with a cutting width of 3 or 4mm are available. In the UK and Ireland, the tools are supplied through the German manufacturer's subsidiary in Ringwood, Hampshire.The M475 system employs precision-ground, indexable inserts with four cutting edges. Positive geometry and a round chip breaker groove together with a new carbide grade, RC4G, deliver economical, productive machining performance. High toughness and hardness enable the machining of steels at elevated cutting speeds and also leads to significantly increased insert life. The cutter bodies are supplied from stock as side, shell and screw-in milling cutters, the two latter variants being equipped for internal coolant supply. Side milling cutters range in diameter from 80mm to 200mm and have cutting widths of 3, 4, 5, 6 or 8mm. As shell mills, the tools are available in diameters from 63mm to 200mm and with identical grooving widths. The screw-in cutters are for a groove width of 5mm and may be ordered in diameters from 40mm to 63mm as standard. The effective number of teeth of depends on tool diameter and ranges from two to 13. Special surface treatment of the tool body offers protection against abrasion from chips.www.phorn.co.uk
Lobsinger explained that the smaller diameter value basically returns the operator back to the original recommended surface speed he is trying to achieve.
With a sophisticated range of high-performance tools, machining solutions provider Walter has been helping customers achieve their efficiency goals for years. Here, the company looks at machining processes in aircraft construction with potential for optimisation.
In celebration of World Space Week, Space-Comm Expo has announced visitor registration is now officially live and open for the London ExCeL, event, running 11-12 March 2025.
The Boeing X-37B spaceplane is to begin executing a series of novel manoeuvres, called aerobraking, to change its orbit around Earth, the US Space Force has announced.
“However, with ceramics, we would recommend opting for a silicon-carbide, whisker-reinforced ceramic insert or a silicon nitride-based ceramic over an alumina-based or white ceramic, as it will provide much more strength and reliability,” said Goss.
Side milling cutters range in diameter from 80mm to 200mm and have cutting widths of 3, 4, 5, 6 or 8mm. As shell mills, the tools are available in diameters from 63mm to 200mm and with identical grooving widths. The screw-in cutters are for a groove width of 5mm and may be ordered in diameters from 40mm to 63mm as standard. The effective number of teeth of depends on tool diameter and ranges from two to 13. Special surface treatment of the tool body offers protection against abrasion from chips.
If you find this article informative, consider subscribing digitally to Aerospace Manufacturing for free. Keep up to date with the latest industry news in your inbox as well as being the first to receive our magazine in digital form.
“When it comes to ceramics, you want to avoid this temptation,” said Lobsinger. “It’s the first thing an operator will do when they start thinking something is going wrong, but you definitely don’t want to do that. The amount of increase in the recommended speed in severely interrupted cuts can usually be calculated. The operator can calculate the circumference of the part, then subtract the total sum of the interruptions. This will give a smaller diameter value, which increases the SFM. Essentially, when increasing cutting speed, you're reducing the time the insert spends out of the cut, thus reducing how much time the insert has to cool, ultimately reducing thermal stress and the growth of the cracks.”
Haid added that it’s always better to start on the low end of the feed rate to provide a bit of wiggle room, rather than running a little bit slow. Running slow can put more impact on the insert.
A rigid setup is necessary for interrupted cuts to take the impact. A round insert is the strongest, followed by a square insert. Dormer Pramet
Some of the impacts of interrupted cuts on the turning process can, depending on the severity of the interruption, lead to accelerated tool wear. This increased tool wear can lead to more tool changes during the process, which ultimately leads to an increase in part cycle times and an overall increase in labour and tooling costs for the job. Here are some factors to consider to help limit tool wear.
Easily access valuable industry resources now with full access to the digital edition of Canadian Fabricating & Welding.
Coolant. The issue of thermal stress leads some operators to believe that running the machine with coolant is the best option.
At the recent AMB 2024 exhibition in Stuttgart, Matthew Farnsworth, commercial director at the University of Sheffield Advanced Manufacturing Research Centre (AMRC) announced that CNC machining centres manufacturer, Heller has become its latest tier 1 member.
An interruption also can be experienced not in the physical sense of material discontinuity, but by an inconsistency in material hardness or having heterogeneity in the material makeup of the workpiece. Goss explained that heterogeneity in the material can occur because of precipitates or inclusions that form during the manufacturing process of the parent material. If these precipitates or inclusions are congregated in one area of the workpiece, they can also act as an interruption during the machining process.
Shape. The experts agree that while different shapes of inserts may work, a round insert is the best option, followed by a square insert.
The impacts of interrupted cuts will depend on the process itself, whether it’s a roughing or finishing application. For the most part, roughing applications tend to include interruptions from forged or cast workpieces that are irregular in material or non-concentric shapes.
Regardless of how a shop classifies interrupted cuts, interruptions can present themselves in a couple of different ways.
With a sophisticated range of high-performance tools, machining solutions provider Walter has been helping customers achieve their efficiency goals for years. Here, the company looks at machining processes in aircraft construction with potential for optimisation.
Babcock International Group (Babcock), the defence company, has been awarded a two-year contract extension by the UK Ministry of Defence (MOD) to continue to provide technical support services across the UK armed forces.
According to John Mitchell, general manager, Tungaloy Canada, Brantford, Ont., carbide cutting tools are made primarily of tungsten, a very hard, wear- resistant material that is bound together with cobalt. To produce a grade capable of handling interrupted cuts, traditionally cutting tool manufacturers simply used more cobalt. On the other hand, to make the insert more wear-resistant, capable of faster cutting speeds and longer tool life, manufacturers used grades that had less cobalt and more tungsten.
Geometry. Another consideration for interrupted cutting is the geometry of the insert. Choosing an insert that has a small nose angle and long, narrow cutting edge does not offer the rigidity needed in most interrupted cutting applications.
For example, a hard grade of carbide will run faster and last longer but is more brittle, whereas a tough grade of carbide has impact resistance but runs slower and does not last as long.
Coating. For interrupted turning, an insert with a physical vapour deposition (PVD) coating on the substrate will help extend tool life. PVD coatings are tougher than chemical vapour deposition (CVD) coatings.
“Tungaloy developed a technology that was able to draw the cobalt to the outer edges of the insert, giving just the cutting edge a higher concentration of cobalt,” said Mitchell. “This allowed for the best of both worlds: a carbide grade with a high concentration of tungsten to allow for higher cutting speeds and longer tool life, while at the same time providing additional concentration of cobalt at the cutting edge to provide additional impact resistance.”
Keep up to date with the latest news, events, and technology for all things metal from our pair of monthly magazines written specifically for Canadian manufacturers!
“If you have the corresponding toolholders in your facility already, a round insert is the strongest,” said Haid. “With a round insert, a rigid setup is necessary to take the impacts of the interrupted cuts. A square insert would be the second strongest. For the most part, diamond-shaped inserts are not well suited, but some interruptions could require a specific insert to get in and perform the cut.”
Lindsay Luminoso, sr. editor/digital editor, contributes to both Canadian Metalworking and Canadian Fabricating & Welding. She worked as an associate editor/web editor, at Canadian Metalworking from 2014-2016 and was most recently an associate editor at Design Engineering.
When you are considering carbide grades, having either a large grain size or cobalt-enriched layer as part of the substrate will make for a stronger insert. Tungaloy
Levels of interrupted cuts can vary anywhere from a light interruption, which might account for only 10 to 20 per cent of the overall process, to a heavy interruption which can be 60 to 75 per cent or more of the overall process. Regardless of how you define interrupted cutting, there are some points to consider when undertaking an interrupted operation.